12-04-09 DEM |
home | solutions | technology | partners | specs | contact. <<< Back InfoDot Performance Specifications Foil Label Test Results >>
Acrylate Label Test Results:
These tests were conducted for a limited period of time
in strict laboratory conditions. In order to achieve maximum satisfaction we
highly recommend that any customer considering using this product test the
labels in the environment in which they will be used.
Heat Test
Adequate contrast ratio for bar code scanning with
intermittent heat exposure to 500 degrees F.
Bar Code Readability Test
This rating measures bar code readability after being
exposed to chemicals listed below for 2 hour soak.
Chemical Emergence tests rated on a scale of 100 to 0: 100 = No Effect 75 = Image Blurred 50 = Image Scratches Off 25 = Image Wipes Off 0 = Image Destroyed Label Adhesion Test
This rating measures label adhesion after being exposed
to chemicals listed below for 2 hour soak.
Chemical emergence tests rated on a scale of 100 to 0: 100 = No Effect 75 = Oozing Adhesion 50 = Label Slides Off 25 = Label Falls Off 0 = Label Destroyed
| |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||